[1]
2016. Ratcheting of 316L stainless steel thin wire under tension-torsion loading. Fracture and Structural Integrity. 10, 38 (Oct. 2016), Pages 141–147. DOI:https://doi.org/10.3221/IGF-ESIS.38.19.